English Chinese Simplified French German Portuguese Spanish Russian Japanese Korean Arabic Irish Greek Turkish Italian Danish Romanian Indonesian Czech Afrikaans Swedish Polish Basque Catalan Esperanto Hindi Lao Albanian Amharic Armenian Azerbaijani Belarusian Bengali Bosnian Bulgarian Cebuano Chichewa Corsican Croatian Dutch Estonian Filipino Finnish Frisian Galician Georgian Gujarati Haitian Hausa Hawaiian Hebrew Hmong Hungarian Icelandic Igbo Javanese Kannada Kazakh Khmer Kurdish Kyrgyz Latin Latvian Lithuanian Luxembou.. Macedonian Malagasy Malay Malayalam Maltese Maori Marathi Mongolian Burmese Nepali Norwegian Pashto Persian Punjabi Serbian Sesotho Sinhala Slovak Slovenian Somali Samoan Scots Gaelic Shona Sindhi Sundanese Swahili Tajik Tamil Telugu Thai Ukrainian Urdu Uzbek Vietnamese Welsh Xhosa Yiddish Yoruba Zulu Kinyarwanda Tatar Oriya Turkmen Uyghur Abkhaz Acehnese Acholi Alur Assamese Awadish Aymara Balinese Bambara Bashkir Batak Karo Bataximau Longong Batak Toba Pemba Betawi Bhojpuri Bicol Breton Buryat Cantonese Chuvash Crimean Tatar Sewing Divi Dogra Doumbe Dzongkha Ewe Fijian Fula Ga Ganda (Luganda) Guarani Hakachin Hiligaynon Hunsrück Iloko Pampanga Kiga Kituba Konkani Kryo Kurdish (Sorani) Latgale Ligurian Limburgish Lingala Lombard Luo Maithili Makassar Malay (Jawi) Steppe Mari Meitei (Manipuri) Minan Mizo Ndebele (Southern) Nepali (Newari) Northern Sotho (Sepéti) Nuer Occitan Oromo Pangasinan Papiamento Punjabi (Shamuki) Quechua Romani Rundi Blood Sanskrit Seychellois Creole Shan Sicilian Silesian Swati Tetum Tigrinya Tsonga Tswana Twi (Akan) Yucatec Maya
Leave Your Message
Aluminium alloy ku hoxa ka ntshikelelo wa le hansi
Mahungu

Aluminum alloy low

AI Helps Write
Swiyenge swa Mahungu
Mahungu Lama Hlamuseriweke

Aluminium alloy ku hoxa ka ntshikelelo wa le hansi

2025-05-06

1. Nkatsakanyo wa thekinoloji ya ku hoxa ya ntshikelelo wa le hansi wa aluminiyamu ya alloy

1.1 Nhlamuselo na nsinya wa nawu

Aluminium alloy low-pressure casting i ya xiyimo xale henhla Thekinoloji ya ku Casting exikarhi ka gravity casting na high-pressure casting. Swipfumelela liquid aluminium alloy kuva yi tlakuka hiku nonoka ehansi ka ntshikelelo naswona yi tata mold cavity ehansi ka ntshikelelo wale hansi (hi ntolovelo 0.02-0.06MPa), kutani yi tiya ehansi ka ntshikelelo. Nsinya wa nawu iku tirhisa ntshikelelo wale hansi ku endla leswaku nsimbi leyi n’okiweke yi tlakuka hiku nonoka ehansi ka ntshikelelo, ku papalata mpfilumpfilu na ku nghenisiwa ka moya hinkarhi wa maendlelo yo tata, leswaku kuta kumeka ti castings letingana xivumbeko xo enta xikan’we na khwalithi ya kahle yale henhla. Thekinoloji leyi yitirhisiwile ngopfu eka tinsimu tofana na timovha na aerospace letingana swilaveko swale henhla swa khwalithi ya casting. Xikombiso, eka vuhumelerisi bya swiphemu swa nkoka swofana na ti cylinder blocks ta njhini ya movha na tinhloko ta cylinder, thekinoloji ya low-pressure casting yinga antswisa swinene swivumbeko swa michini xikan’we naku pakanisa ka dimensional ya ti castings xikan’we naku hunguta ti scrap rates.

2. Ku khuluka ka phurosese na tipharamitha ta nkoka

2.1 Ku hahluka ka ku khuluka ka phurosese

Ku khuluka ka maendlelo ya aluminium alloy low-pressure casting ngopfu ngopfu swikatsa magoza lawa ya landzelaka:

Xiyenge xo lunghiselela: Xo sungula, xivumbeko xi fanele xi hisiwa ka ha ri emahlweni. Mahiselo ya preheating yatala kuva exikarhi ka 200-300°C kutiyisisa leswaku nsimbi leyi n’okiweke yinga hatli yi hola hinkarhi wa maendlelo yo tata hikokwalaho ka mahiselo yale hansi ya mold, leswinga ta khumba mbuyelo wo tata. Hi nkarhi lowu fanaka, nsimbi leyi n’okiweke ya antswisiwa leswaku ku susiwa thyaka na tigasi ku tiyisisa ku basa ka nsimbi leyi n’okiweke. Xikombiso, hiku tirhisa switirhisiwa swo basisa na switirhisiwa swo susa gasi, nhlayo ya hydrogen eka nsimbi leyi n’okiweke yinga hungutiwa kuya ehansi ka 0.1-0.2ml/100gAl, kahle kahle swihunguta swihoxo swa porosity eka casting.

Xiyenge xo tata: Xivumbeko lexi hisiweke ka ha ri emahlweni xi vekiwa eka muchini wo hoxa hi ntshikelelo wa le hansi, ivi nsimbi leyi n’okiweke yi cheriwa ku suka eka khapu yo chela eka riser. Ehansi ka xiendlo xa ntshikelelo wale hansi, nsimbi leyi n’okiweke yi tlakuka hiku nonoka kuya hi riser naswona yi tata ndzhawu yo hoxa. Rivilo ro tata hi xitalo rilawuriwa eka 0.05-0.2m/s kutiyisisa leswaku nsimbi leyi n’okiweke yi tlakuka hiku olova naswona yi papalata mpfilumpfilu xikan’we naku nghenisiwa ka moya. Xikombiso, loko ku endliwa ti cylinder blocks ta njhini ya movha, hiku lawula kahle rivilo ro tata, khwalithi yale henhla ya casting yinga fika eka Ra0.8 - 1.6μm, ku fikelela swilaveko swa khwalithi ya indasitiri ya mimovha.

Xiteji xa solidification: Endzhaku kaloko nsimbi leyi n’okiweke yi tatile xivandla, yana emahlweni u hlayisa ntshikelelo wo karhi ku tiyisisa casting ehansi ka ntshikelelo. Nkarhi wo tiya wuya hi vukulu na xivumbeko xa casting, hi xitalo kusuka eka timinete nyana kuya eka kutlula khume ra timinete. Hi nkarhi wa maendlelo ya solidification, ku hlayisiwa ka ntshikelelo swi pfuna nsimbi leyi n’okiweke ku engetela ku hunguteka na ku hunguta swihoxo swa ku hunguteka na ku hunguteka. Xikombiso, eka ti aerospace castings letikulu, nkarhi wa solidification wunga leha kufika eka 30-40 wa timinete kutiyisisa leswaku xivumbeko xale ndzeni xa casting xi tsindziyerile.

Xiteji xo pfula na ku susa xivumbeko: Endzhaku ka loko casting yi tiyile, tshika ku chela ntshikelelo, pfula mold, kutani u susa casting. Hi nkarhi lowu, mahiselo ya casting yahari e henhla, naswona vutshunguri lebyi faneleke byo kufumeta, kufana na ku kufumeta hi moya kumbe ku kufumela ka mati, swa laveka kuva ku sivela casting kuva yi onhaka kumbe ku pandzeka hinkarhi wa maendlelo yo kufumeta. Hi xikombiso, eka swilo swin’wana leswi nga ni marhangu yo olova, ku kufumela ka moya ku nga papalata ku pandzeka loku vangiwaka hi rivilo lerikulu ro kufumela.

2.2 Vulawuri bya parameter ya xilotlelo

Eka endlelo ra aluminium alloy low-pressure casting, vulawuri bya ti parameters ta nkoka byi na nkucetelo wa nkoka eka khwalithi ya ti castings:

Ku lawula ntshikelelo: Ntshikelelo wa low-pressure casting i yin’wana ya ti core parameters leti khumbhaka khwalithi ya ti castings. Hi ntolovelo yi avanyisiwile hi ntshikelelo wo tata na ntshikelelo wo khoma. Ntshikelelo wo tata wutala ku lawuriwa eka 0.02-0.06MPa, naswona ntshikelelo wo khoma wu lulamisiwa kuya hi vukulu na ku rharhangana ka casting, hi xitalo exikarhi ka 0.05-0.1MPa. Xikombiso, loko ku endliwa ti cylinder heads ta njhini ya movha, ntshikelelo wo tata wu hlawuriwa kuva wuva 0.04MPa naswona ntshikelelo wo khoma wuva 0.08MPa, leswinga tiyisisaka kahle vutshembeki byo tata na khwalithi yale ndzeni ya casting naswona swiendla leswaku density ya casting yifika kutlula 98%.

Ku lawula mahiselo: kukatsa na mahiselo ya nsimbi leyi n’okiweke na mahiselo ya xivumbeko. Mahiselo ya nsimbi leyi n’okiweke hi xitalo ya lawuriwa eka 650-750°C. Mahiselo yale henhla swinene yata endla leswaku kuva na oxidation xikan’we naku hefemula ka moya eka nsimbi leyi n’okiweke, naswona mahiselo yale hansi swinene yata khumba mbuyelo wo tata. Mahiselo ya mould yatala ku hisiwa kuya eka 200-300°C naswona yatshama yatshamisekile swinene hinkarhi wa vuhumelerisi. Hi xikombiso, loko u humesa Ku Hoxiwa ka Aluminium Alloys eka aerospace, swivumbeko swa michini swa ti castings swinga antswisiwa swinene hiku lawula kahle mahiselo ya nsimbi leyi n’okiweke xikan’we na mahiselo ya mould, na matimba ya tensile ya 300-350MPa xikan’we naku leha ka 3%-5%.

Ku lawula rivilo ro tata: Ku lawula loku ringaneleke ka rivilo ro tata swinga papalata mpfilumpfilu na ku nghenisiwa ka moya eka nsimbi leyi n’okiweke hi nkarhi wa ku tata. Hi xitalo yi lawuriwa hi 0.05-0.2m/s. Xikombiso, loko ku endliwa mavhilwa ya movha, hiku antswisa rivilo ro tata, khwalithi yale henhla ya casting yinga fika eka Ra1.6-3.2μm, loko kurikarhi kuhungutiwa ku tumbuluxiwa ka ti pore defects xikan’we naku antswisa khwalithi hinkwayo ya casting.

Ku lawula nkarhi wa ku tiya: Ku leha ka nkarhi wa ku tiya swi khumba hiku kongoma khwalithi yale ndzeni xikan’we naku pakanisa ka dimensional ya casting. Eka ti castings letintsongo, nkarhi wa solidification hi ntolovelo i timinete nyana; eka ti castings letikulu, nkarhi wo tiya wunga leha kufika eka khume ra timinete kumbe hambi kuri ku tlula. Xikombiso, loko ku humelerisiwa ti aerospace castings letikulu, hiku engetela nkarhi wa solidification kuya eka 30-40 wa timinete, swihoxo swa shrinkage na shrinkage swinga hungutiwa hindlela leyinene, leswi endlaka leswaku xivumbeko xale ndzeni xa casting xiva na denser xikan’we na dimensional accuracy endzeni ka ±0.5mm.

3. Swilaveko swa switirhisiwa na xivumbeko

3.1 Swihlawulekisi swa switirhisiwa swo hoxa swa ntshikelelo wa le hansi

Switirhisiwa swo hoxa swa ntshikelelo wa le hansi wa aluminiyamu i xitirhisiwa xa nkoka xo lemuka endlelo ro hoxa hi ntshikelelo wa le hansi, naswona dizayini ya yona na matirhelo ya yona swi khumba hi ku kongoma khwalithi na vuhumelerisi bya kahle bya ku hoxa.

Endlelo ro lawula ntshikelelo: Switirhisiwa leswi swi hlomisiwile hi sisiteme ya vulawuri bya ntshikelelo ya vukheta lebyikulu leyi nga lawulaka kahle ntshikelelo wo tata na ntshikelelo wo khoma. Xikombiso, ku lulama ka vulawuri bya ntshikelelo wa michini ya manguva lawa yo hoxa ya ntshikelelo wale hansi swinga fika eka ±0.001MPa, leswi tiyisisaka leswaku nsimbi leyi n’okiweke yinga tlakuka hiku olova hinkarhi wa maendlelo yo tata ku papalata mpfilumpfilu xikan’we naku nghenisiwa ka moya. Vulawuri lebyi bya ntshikelelo bya kahle swinene i bya nkoka eka vuhumelerisi bya ti castings ta xiyimo xale henhla to rharhangana tofana na ti cylinder blocks ta njhini ya movha.

Endlelo ro lawula mahiselo: Switirhisiwa leswi swi hlomisiwile hi endlelo ro lawula mahiselo leri tirhaka kahle leri nga lawulaka mahiselo ya nsimbi leyi n’okiweke na mahiselo ya xivumbeko hi nkarhi wun’we. Ku lulama ka vulawuri bya mahiselo ya nsimbi leyi n’okiweke switala kuva endzeni ka ±5°C, naswona ku lulama ka preheating naku khoma ka mahiselo ya mold swile ndzeni ka ±10°C. Xikombiso, loko ku endliwa ti aluminium alloy castings ta aerospace, vulawuri bya mahiselo lebyi kongomeke byi nga antswisa swinene swivumbeko swa michini swa ti castings, laha matimba ya tensile ya fikaka eka 300-350MPa naswona elongation yifika eka 3%-5%.

Automation: Switirhisiwa swa manguva lawa swa low-pressure casting swi automated swinene naswona swinga lemuka endlelo hinkwaro ra automated operation kusuka eka ku cheriwa ka mati ya nsimbi, ku tata mold, solidification kuya eka ku pfula mold naku humesa swiphemu. Ku antswisiwa ka automation aswi antswisi ntsena vuhumelerisi bya kahle, kambe switlhela swihunguta mbuyelo wa swilo swa vanhu eka khwalithi ya casting. Xikombiso, vuhumelerisi bya kahle bya switirhisiwa swa automated byi le henhla hi 30%-50% kutlula bya ndhavuko wa manual operation, naswona scrap rate ya ti castings yihungutiwile kuya eka 2%-3%.

Ku tirha ka vuhlayiseki: Switirhisiwa swo hoxa swa ntshikelelo wa le hansi swi endliwile hi ku tekela enhlokweni hi ku hetiseka vuhlayiseki bya ntirho. Switirhisiwa leswi swi hlomisiwile hi switirhisiwa swa vuhlayiseki swo fana na xitirhisiwa xo yima hi xihatla, nyangwa wo sirhelela vuhlayiseki na sisiteme yo kuma ku vupfa. Xikombiso, nyangwa wa nsirhelelo wa vuhlayiseki wa xitirhisiwa wu pfala hi woxe hi nkarhi wa ntirho ku sivela mati ya nsimbi ku khuluka na ku vavisa vanhu, naswona sisiteme yo kuma ku vupfa yi nga languta ntshikelelo na mahiselo endzeni ka xitirhisiwa hi nkarhi wa xiviri ku tiyisisa vuhlayiseki bya endlelo ro tirha.

3.2 Dizayini ya xivumbeko na ku hlawuriwa ka switirhisiwa

Mold i xiphemu xa nkoka eka maendlelo ya low-pressure casting, naswona dizayini ya yona xikan’we naku hlawuriwa ka switirhisiwa swina nkucetelo wa nkoka eka khwalithi na ntsengo wa vuhumelerisi bya casting.

Dizayini ya xivumbeko: Dizayini ya xivumbeko yi fanele ku kambisisa hi vuenti swilo swo tanihi xivumbeko, vukulu ni ku enta ka rirhangu ra xirhendzevutani. Hi xikombiso, eka xivumbeko lexi rharhanganeke xa nhloko ya silindara ya njhini ya movha, pulani ya xivumbeko yi amukela xivumbeko xa block ku olovisa ku susiwa ka xivumbeko xa casting na ku hlayisiwa ka xivumbeko. Hi nkarhi walowo, dizayini ya mould yitlhela yilava ku tekela enhlokweni ndlela yo khuluka ya nsimbi leyi n’okiweke, naku hunguta swihoxo swa ti pores na slag inclusions hiku antswisa dizayini ya gede na exhaust system. Xikombiso, dizayini ya xivumbeko lexi antswisiweke yinga endla leswaku khwalithi yale henhla ya casting yifika eka Ra0.8 - 1.6μm, leswi fikelelaka swilaveko swa khwalithi ya indasitiri ya mimovha.

Ku hlawula swilo: Switirhisiwa swa xivumbeko hi ntolovelo swi endliwa hi nsimbi ya alloy leyi nga ni matimba swinene, leyi nga ni mahiselo lamakulu ni leyi nga onhakiki. Xikombiso, nsimbi ya H13 i xitirhisiwa xa xivumbeko lexi tirhisiwaka ngopfu lexinga na ku tiya kahle ka mahiselo xikan’we naku lwisana na ku karhala ka mahiselo, naswona yinga tiyisela ku phindha-phindha ka thermal shock xikan’we na ntshikelelo wa michini. Loko ku humelerisiwa ti aerospace castings letikulu, vutomi bya vutirheli bya mould material byinga fika eka 10,000 - 15,000 times, kahle kahle swihunguta ntsengo wa vuhumelerisi.

Ku basisiwa ka le henhla: Vuandlalo bya xivumbeko hi ntolovelo byi endliwa hi ndlela yo hlawuleka, kufana na hard chrome plating, nitriding, na swin’wana, ku antswisa ku tiya ka ku onhaka xikan’we naku tiya ka xivumbeko xa corrosion. Xikombiso, ku tiya ka le henhla ka xivumbeko endzhaku ka hard chrome plating swinga engeteriwa kuya eka HRC60-65, naswona vutomi bya ntirho byinga engeteriwa hi 20%-30%. Hi nkarhi lowu fanaka, xiendlakalo xa ku namarhela ehenhla ka casting swa hunguteka, naswona khwalithi ya le henhla ya casting ya antswisiwa.

Ku lulama ka vumaki bya xivumbeko: Ku lulama ka vumaki bya xivumbeko swi khumba hi ku kongoma ku pakanisa ka dimensional na khwalithi ya le henhla ya casting. Vumaki bya manguva lawa bya xivumbeko byi tirhisa switirhisiwa swa michini swa CNC swa vukheta bya le henhla, naswona ku pakanisa ka dimensional ya mould kunga fika eka ±0.05mm, naswona ku khwaxa ka le henhla kunga lawuriwa endzeni ka Ra0.4-0.8μm. Xikombiso, loko ku endliwa mavhilwa ya mimovha, vumaki bya xivumbeko xa kahle swinene byi nga endla leswaku ku pakanisa ka dimensional ka casting ku fikelela endzeni ka ±0.1mm naswona khwalithi ya le henhla yi fika eka Ra1.6-3.2μm, ku fikelela xilaveko xa makete xa ti castings ta xiyimo xa le henhla.

4. Swipfuno na Tinsimu ta ku Tirhisa

4.1 Nxopaxopo wa Swipfuno swa Maendlelo

Loko ku pimanyisiwa na maendlelo ya ndhavuko yo hoxa, thekinoloji ya aluminium alloy low-pressure casting yina swipfuno leswikulu swa maendlelo, leswi endlaka leswaku yitsakeriwa eka vumaki bya manguva lawa.

Ti castings ta xiyimo xale henhla: Thekinoloji ya low-pressure casting kahle kahle yi papalata mpfilumpfilu xikan’we naku nghenisiwa ka moya wa nsimbi leyi n’okiweke hinkarhi wa maendlelo yo tata hiku tata hiku olova naku tiya ehansi ka ntshikelelo eka ntshikelelo wale hansi, leswi hungutaka swihoxo swofana na ti pores, kuhunguteka naku hunguteka eka ti castings. Xikombiso, density ya ti cylinder blocks ta njhini ya movha leti humelerisiwaka hi low-pressure casting yinga fika kutlula 98%, swivumbeko swa michini swi antswisiwile swinene, matimba ya tensile ya fika eka 300-350MPa, elongation yifika eka 3%-5%, naswona scrap rate yihungutiwile kuya eka 2%-3%.

Ku lulama ka dimensional yale henhla: Endlelo leri ringa lawula kahle rivilo ro tata na nkarhi wo tiya ku tiyisisa ku pakanisa ka dimensional ya casting. Xikombiso, loko ku humelerisiwa ti aerospace castings letikulu, hiku engetela nkarhi wa solidification kuya eka 30-40 wa timinete, dimensional accuracy ya casting yinga fika endzeni ka ±0.5mm, ku fikelela swilaveko swale henhla swa precision.

Ku tirha kahle ka vuhumelerisi byale henhla: Switirhisiwa swa manguva lawa swo hoxa swa ntshikelelo wale hansi swi endliwa hi xiothomethi swinene naswona swinga lemuka endlelo hinkwaro ra ntirho wa xiothomethi kusuka eka ku cheriwa ka mati ya nsimbi, ku tata xivumbeko, ku tiya kuya eka ku pfula ka xivumbeko na ku humesa swiphemu. Kuhumelela ka vuhumelerisi bya switirhisiwa swa automated swile henhla hi 30% - 50% kutlula swa ndhavuko wa manual operation, loko kurikarhi kuhungutiwa nkucetelo wa swilo swa vanhu eka khwalithi ya ti castings.

Mpimo wa le henhla wa ku tirhisiwa ka swilo: Hi nkarhi wa endlelo ro hoxa hi ntshikelelo wa le hansi, nsimbi leyi n’okiweke yi tlakuka hakatsongo-tsongo naswona yi tata xirhendzevutana ehansi ka ntshikelelo, leswi hungutaka ku khuluka ni ku tlangisiwa ka nsimbi leyi n’okiweke. Xikombiso, loko ku endliwa mavhilwa ya mimovha, mpimo wa matirhiselo ya swilo wunga engeteriwa hi 15% - 20%, leswi hungutaka ku durha ka vuhumelerisi.

Ku cinca cinca loku tiyeke: Endlelo leri ri lulamerile eka vuhumelerisi bya ti castings ta switirhisiwa swohambana hambana swa aluminium alloy na swivumbeko leswi rharhanganeke, kusuka eka ti castings ta marhangu yo olova kuya eka ti castings letikulu ta marhangu yo tiya. Hi xikombiso, eka mavhilwa ya timovha lama nga ni marhangu yo olova ni swilo leswikulu leswi hoxiweke exibakabakeni, ku hoxa ka ntshikelelo wa le hansi ku nga fikelela swilaveko swa wona swa khwalithi ni swa matirhelo.

4.2 Ku ndlandlamuxiwa ka tinsimu ta matirhiselo

Thekinoloji ya aluminium alloy low-pressure casting yitirhisiwile ngopfu eka tinsimu totala hikokwalaho ka swipfuno swa yona swo hlawuleka, naswona swiletelo swintshwa swa matirhiselo switshama swiri karhi swi ndlandlamuxiwa.

Indasitiri ya mimovha: Swiphemu swa nkoka swofana na ti cylinder blocks ta njhini ya timovha na tinhloko ta ti cylinder i swilo leswikulu leswi tirhisiwaka eka thekinoloji ya low-pressure casting. Xikombiso, kutlula 70% wa vaendli va timovha va misava hinkwayo va tirhisa thekinoloji ya low-pressure casting ku humesa ti cylinder blocks ta njhini, naswona ku antswisiwa ka khwalithi ya ti castings ta vona hiku kongoma swi antswisa matirhelo na ku tshembheka ka njhini. Ku engetela kwalano, low-pressure casting yitlhela yitirhisiwa ngopfu eka vuhumelerisi bya mavhilwa ya timovha, leswinga antswisiki ntsena matimba na levele yo olova ya mavhilwa, kambe switlhela swihunguta ku durha ka vuhumelerisi.

Nsimu ya aerospace: Nsimu ya aerospace yina swilaveko swale henhla swinene swa khwalithi na matirhelo ya ti castings, naswona thekinoloji ya low-pressure casting yinga fikelela swilaveko swa yona leswi lavaka. Xikombiso, loko ku humelerisiwa ti aerospace castings letikulu, thekinoloji ya low-pressure casting yinga endla leswaku xivumbeko xale ndzeni xa ti castings xiva lexi ringanaka, ku pakanisa ka dimensional kunga fika endzeni ka ±0.5mm, naswona swivumbeko swa michini swiantswisiwile swinene. Kuya hi tinhlayo, ti aerospace castings leti humelerisiwaka hi low-pressure casting ti endla kutlula 40% wa ti castings hinkwato eka ntirho lowu, naswona xiphemu lexi xaha kula.

Indasitiri ya swithuthuthu: Thekinoloji ya low-pressure casting yitlhela yitirhisiwa ngopfu eka vuhumelerisi bya ti cylinder blocks ta njhini ya swithuthuthu, tinhloko ta cylinder na mavhilwa na swiphemu swin’wana. Xikombiso, muendli wa swithuthuthu loyi a tivekaka swinene u tirhisa thekinoloji ya low-pressure casting ku humelerisa ti cylinders ta njhini, naswona nhlayo ya switirhisiwa swa yena swa scrap yihungutiwile kuya eka 2% - 3%, naswona vukorhokeri bya vuhumelerisi byi engeteriwile hi 30% - 50%, leswi antswisaka swinene mphikizano wa makete wa khamphani.

Indasitiri ya vumaki bya michini: Eka xiyenge xa ​​vumaki bya michini, thekinoloji ya low-pressure casting yitirhisiwa ku humelerisa ti aluminium alloy castings letingana swivumbeko swohambana hambana leswi rharhanganeke na swilaveko swa matirhelo yale henhla, kufana na mimiri ya ti valve ta hayidiroliki, mimiri ya pompo, etc. Xikombiso, khamphani yo endla michini yi tirhisa thekinoloji ya low-pressure casting ku humelerisa mimiri ya ti valve ta hydraulic, naswona density ya ti castings ta yona ya tlakuka ku tlula 98%, swivumbeko swa michini swi antswisiwile swinene, naswona vutomi bya vukorhokeri byi engeteriwile hi 20% - 30%.

Tinsimu ta matirhiselo leti humelelaka: Hi nhluvuko lowu yaka emahlweni wa thekinoloji, thekinoloji ya aluminiyamu ya alloy ya ntshikelelo wa le hansi wa ku hoxa yi tlhele yi kombisa ntshembo wo anama wa matirhiselo eka tinsimu leti hluvukaka to fana na mimovha leyintshwa ya eneji na switirhisiwa swa vuhlanganisi swa 5G. Xikombiso, eka vuhumelerisi bya swikhegelo swa tibetiri na tindlu ta timovha ta mimovha leyintshwa ya eneji, thekinoloji ya ku hoxa hi ntshikelelo wa le hansi yi nga fikelela swilaveko swa yona swo vevuka na matirhelo ya le henhla, na ku antswisa matirhelo hinkwawo na ku tiyisela ka mimovha leyintshwa ya eneji.

5. Ku lawula khwalithi na ku sivela swihoxo

5.1 Maendlelo yo kambela khwalithi

Ku kamberiwa ka khwalithi ya aluminium alloy low-pressure casting i xihlanganisi xa nkoka ku tiyisisa leswaku ti castings ti fikelela swipimelo. Ku tirhisiwa ngopfu tindlela leti landzelaka:

Ku kamberiwa loku nga onhiki: ku katsa na ku kamberiwa ka ultrasonic, ku kamberiwa ka radiographic (ku fana na X-ray na CT scanning) na ku kamberiwa ka ti magnetic particle. Ku kamberiwa ka ultrasonic swinga vona swihoxo swofana na ku pandzeka na ti shrinkage holes endzeni ka ti castings hiku pakanisa ka ku vona kuya fika eka levele ya millimeter; ku kamberiwa ka radiographic swinga kombisa hindlela yo twisiseka xivumbeko xale ndzeni xa ti castings, naswona swina mbuyelo lowukulu eka ku kumiwa ka swihoxo swale ndzeni swa ti castings ta xivumbeko xo rharhangana; magnetic particle testing yitirhisiwa ngopfu ku kuma swihoxo swofana na ku pandzeka ehenhla kumbe ekusuhi na le henhla. Xikombiso, eka xiyenge xa ​​aerospace, CT scanning ya ti castings letikulu ta aluminium alloy yinga vona ti pores tale ndzeni nati inclusions letingana diameter yale hansi ka 0.5mm, leswi tiyisisaka khwalithi yale henhla ya ti castings.

Ku kambela hi ti dimensions: Tirhisa switirhisiwa swofana na switirhisiwa swo pima swa three-coordinate na ti laser scanners ku kambela ku pakanisa ka dimensional ya ti castings. Ku lulama ka ku pima ka muchini wo pima wa swiphemu swinharhu swinga fika eka ±0.01mm, leswinga pima kahle swipimelo swale handle na swipimelo swa xivumbeko xale ndzeni xa casting; xikeni xa laser xi nga hatlisa xi kuma datha ya tidimenxini ta swiphemu swinharhu swa casting, xi yi pimanisa na modele wa dizayini, na ku vona ku hambuka ka tidimenxini. Xikombiso, eka vuhumelerisi bya ti cylinders ta njhini ya movha, muchini wo pima wa swiphemu swinharhu wu tirhisiwa ku kuma swipimelo swa nkoka swa miri wa silindara kufana na bore diameter na hole spacing kutiyisisa leswaku ku pakanisa ka yona kule ndzeni ka ±0.05mm kuva yi fikelela swilaveko swa nhlengeletano.

Ku kamberiwa ka swivumbeko swa michini: Swihlawulekisi swa michini swa ti castings swi kamberiwa hi swikambelo swa tensile, swikambelo swa ku tiya na tindlela tin’wana. Xikambelo xa tensile xinga kumisisa matimba ya tensile, matimba ya yield xikan’we naku leha ka casting; xikambelo xa ku tiya xi tirhisiwa ku kambela ku hangalaka ka ku tiya ehenhla na le ndzeni ka casting. Xikombiso, eka mavhilwa ya aluminium alloy lawa ya humelerisiwaka hi low-pressure casting, mbuyelo wa tensile test wukombisa leswaku matimba ya yona ya tensile yanga fika eka 280-320MPa, elongation i 3%-5%, naswona mbuyelo wa hardness test wukombisa leswaku surface hardness ya yona yile xikarhi ka HRC30-35, leswi fikelelaka swilaveko swa matirhiselo.

Nxopaxopo wa metallographic: Languta microstructure ya casting hiku tirhisa metallographic microscope kuva u kambisisa swihlawulekisi swofana na vukulu bya mavele na xivumbeko xa phase. Nxopaxopo wa metallographic wunga paluxa swiphiqo leswinga humelelaka hinkarhi wa solidification process ya casting, kufana na coarse grains xikan’we naku hambanisiwa. Xikombiso, loko ku endliwa ti aluminium alloy castings ta aerospace, nxopaxopo wa metallographic wukombisa leswaku vukulu bya mavele byi lawuriwa exikarhi ka 50-100μm, xivumbeko xafana, naswona akuri na ku hambanisiwa loku vonakaka, leswi pfunetaka ku tiyisisa matirhelo yale henhla ya casting.

5.2 Swihoxo leswi tolovelekeke na magoza yo sivela

Kuna swihoxo swotala leswinga humelelaka hi nkarhi wa low-pressure casting ya aluminium alloys. Swihoxo leswi aswi khumbi ntsena khwalithi ya xivumbeko xa ti castings, kambe swinga tlhela swihunguta swivumbeko swa tona swa michini xikan’we na vutomi bya ntirho. Leswi landzelaka i swihoxo leswi tolovelekeke na magoza ya swona yo sivela:

Porosity defect: Porosity i xin’wana xa swihoxo leswi tolovelekeke eka low-pressure casting ya aluminium alloys, ngopfu ngopfu swivangiwa hiku khomiwa ka gasi eka nsimbi leyi n’okiweke hinkarhi wa ku tata kumbe ku humesiwa ka mould lokunga kahle. Magoza yo sivela ma katsa:

Antswisa rivilo ro tata naswona ri lawula eka 0.05-0.2m/s ku papalata mpfilumpfilu na ku nghenisiwa ka nsimbi leyi n’okiweke.

Tiyisisa leswaku sisiteme yo humesa moya ya xivumbeko a yi kavanyetiwi, naswona hi ndlela leyi twalaka dizayina ndhawu na vukulu bya groove yo humesa moya na khumbi ro humesa moya.

Hlawula nsimbi leyi n’okiweke hiku hetiseka kuva u susa thyaka na tigasi, naswona u lawula nhlayo ya hydrogen ehansi ka 0.1-0.2ml/100gAl.

Hlayisa mahiselo ya mold eka 200-300°C, hunguta ku kufumela ka nsimbi leyi n’okiweke hinkarhi wa ku tata, naswona papalata ku khuluka ka gasi kuva yi endla ti pores.

Xikombiso, eka vuhumelerisi bya ti cylinders ta njhini ya movha, hiku antswisa rivilo ro tata na dizayini ya exhaust system, pore defect rate yihungutiwile kutlula 50%, naswona density ya casting yi antswisiwile swinene.

Swihoxo swa kuhunguteka naku hunguteka: Swihoxo leswi swivangiwa hiku pfumaleka ka shrinkage compensation hikokwalaho ka volume shrinkage ya nsimbi leyi n’okiweke hinkarhi wa solidification. Magoza yo sivela ma katsa:

Lawula hindlela leyinene ntshikelelo wo khoma xikan’we na nkarhi wa solidification kutiyisisa leswaku nsimbi leyi n’okiweke yinga tlherisela hiku hetiseka ku hunguteka hinkarhi wa maendlelo ya solidification. Xikombiso, eka ti aerospace castings letikulu, ntshikelelo wo khoma wu hlawuriwa kuva wuva 0.08-0.1MPa, naswona nkarhi wa solidification wu engeteriwa kuya eka 30-40 wa timinete, leswinga hunguta kahle ku hunguteka na swihoxo swa shrinkage.

Ku antswisa dizayini ya xivumbeko xa ti castings ku papalata ku hunguteka loku hlanganisiweke eka swiphemu swo tiya na leswikulu, naswona amukela endlelo ro chela leri ringaneleke na dizayini ya riser ku tiyisisa ku tiya hi ku landzelelana ka nsimbi leyi n’okiweke.

Lawula swinene mahiselo ya nsimbi leyi n’okiweke xikan’we na mahiselo ya mold kuva ku papalata oxidation xikan’we naku hefemula ka moya wa nsimbi leyi n’okiweke hikokwalaho ka mahiselo yotala, leswinga ta khumba mbuyelo wa shrinkage compensation.

Xikombiso, eka vuhumelerisi bya mavhilwa ya timovha, hiku antswisa ntshikelelo wo khoma na nkarhi wo tiya, xivandla xa shrinkage na shrinkage defect rate swihungutiwile hi 40%, naswona xivumbeko xale ndzeni xa casting axiri xitsongo swinene.

Slag inclusion defect: Slag inclusion yivumbiwa loko thyaka kumbe oxide scale eka nsimbi leyi n’okiweke yi rhendzeleka eka casting hinkarhi wa maendlelo yo tata. Magoza yo sivela ma katsa:

Hlawula nsimbi leyi n’okiweke hiku hetiseka kuva u susa thyaka xikan’we na oxide scale kutiyisisa ku basa ka nsimbi leyi n’okiweke.

Endla kahle dizayini ya sisiteme yo chela ku papalata mpfilumpfilu na slag rolling ya nsimbi leyi n’okiweke hinkarhi wa maendlelo yo tata.

Lawula hindlela leyinene rivilo ro chela na rivilo ro tata ku tiyisisa leswaku nsimbi leyi n’okiweke yi tlakuka hiku olova naswona yi hunguta ku koteka ka ku katsa slag.

Tirhisa switirhisiwa swo sefa swofana na ti filter screens kuva u sefa nsimbi leyi n’okiweke kuva u susa swiphemu leswikulu swa thyaka na oxide scale.

Xikombiso, eka vuhumelerisi bya mavhilwa ya aluminium alloy, mpimo wa xihoxo xa ku katsa slag wu hungutiwile hi 30% hiku tirhisa filtara naku antswisa dizayini ya sisiteme yo chela, naswona khwalithi yale henhla na khwalithi yale ndzeni ya ti castings swi antswisiwile swinene.

Swihoxo swale henhla: kufana na ku khwaxa ka le henhla, ku pfala hi xirhami, swikombiso swa ku khuluka, na swin’wana na swin’wana Swihoxo leswi ngopfu ngopfu swi khumba khwalithi ya xivumbeko xikan’we naku pakanisa ka dimensional ya ti castings. Magoza yo sivela ma katsa:

Endla leswaku rivilo ro tata xikan’we na mahiselo ya mold kutiyisisa leswaku nsimbi leyi n’okiweke yinga tlakuka hiku olova hinkarhi wa maendlelo yo tata naswona ku papalata swikoweto swo pfala hi xirhami xikan’we naku khuluka.

Hlayisa vuandlalo bya xivumbeko byi basile naswona byi ri eka xiyimo xa kahle xa mafurha, hunguta ku namarhela ka nsimbi leyi n’okiweke eka vuandlalo bya xivumbeko, naswona u antswisa khwalithi ya le henhla ya casting.

Lawula swinene ku basa ka nsimbi leyi n’okiweke ku papalata nkucetelo wa thyaka na gasi eka khwalithi yale henhla ya casting.

Tirhisa switirhisiwa swo endla xivumbeko xa vukheta bya le henhla ku tiyisisa leswaku ku pakanisa ka dimensional na ku khwaxa ka vuandlalo bya xivumbeko swi fikelela swilaveko.

Xikombiso, eka vuhumelerisi bya tinhloko ta ti cylinder ta njhini ya movha, hiku antswisa rivilo ro tata na mahiselo ya mould, ku khwaxa ka le henhla swinga lawuriwa eka Ra0.8 - 1.6μm, cold shut na flow mark defect rate swihungutiwile hi 60%, naswona khwalithi ya xivumbeko xa casting yi antswisiwile swinene.

6. Mikhuva ya Nhluvukiso na Vumaki bya Thekinoloji

6.1 Mikhuva ya Nhluvukiso wa Thekinoloji

Thekinoloji ya aluminium alloy low-pressure casting yi le ku hluvukeni eka matlhelo yo tala ku fikelela xilaveko xa makete lexi kulaka na swilaveko swa khwalithi ya le henhla.

Vutlhari na otomatiki swi ya emahlweni swi antswisiwa: Hi ku ya emahlweni ka Indasitiri 4.0, vutlhari na mpimo wa otomatiki wa switirhisiwa swo hoxa swa ntshikelelo wa le hansi swi ta antswisiwa ku ya emahlweni. Xikombiso, hiku nghenisa thekinoloji ya xiyimo xale henhla ya switwi na tisisiteme ta vulawuri bya otomatiki, ku vekiwa tihlo ka nkarhi wa xiviri na vulawuri lebyi kongomeke bya endlelo ro hoxa swinga fikeleriwa, kukatsa na ku lulamisiwa ka otomatiki ka ti parameter ta nkoka tofana na ntshikelelo, mahiselo, na rivilo ro tata. Leswi aswinga antswisi ntsena vuhumelerisi bya kahle, kambe switlhela swihunguta kuya emahlweni nhlayo ya scrap xikan’we naku antswisa kutshamiseka ka khwalithi ya casting.

Ku hoxa ka rihlaza na ku hlayisa eneji na ku hunguta ku tirhisiwa: Hi ku ya hi ku tlakuka ka vutivi bya mbango bya misava hinkwayo, thekinoloji ya ku hoxa hi ntshikelelo wa le hansi yi ta nyikela nyingiso lowukulu eka nhluvukiso wa rihlaza. Hi tlhelo rin’we, hi ku antswisa tipharamitha ta phurosese na dizayini ya switirhisiwa, ku tirhisiwa ka eneji na ku humesiwa ka moya swi nga hungutiwa; hi hala tlhelo, ku tirhisiwa swilo leswi nga onhiki mbango ni swilo swo peta mbango leswaku ku hunguta ku thyakisa mbango. Xikombiso, michini yin’wana leyintshwa leyi hlayisaka eneji ya low-pressure casting yinga hunguta ku tirhisiwa ka eneji hi 20% - 30% hiku antswisa tisisiteme to kufumeta na magoza ya insulation.

Ku tirhisiwa ka switirhisiwa swa aluminiyamu swa matirhelo ya le henhla: Leswaku ku fikeleriwa swilaveko swa le henhla swa matirhelo ya ku hoxa eka tinsimu ta xiyimo xa le henhla to fana na mimovha ya swihahampfhuka na ya eneji leyintshwa, ndzavisiso na nhluvukiso na ku tirhisiwa ka switirhisiwa swa aluminiyamu swa matirhelo ya le henhla swi ta va nhlokomhaka ya nhluvukiso wa nkarhi lowu taka. Xikombiso, hiku engetela swiaki swokarhi swa alloying xikan’we naku antswisa maendlelo ya vutshunguri bya kuhisa, switirhisiwa swa aluminium alloy leswingana matimba yale henhla, ku tiya xikan’we naku lwisana na corrosion swi tumbuluxiwile ku ya emahlweni swi ndlandlamuxa xikalo xa ku tirhisiwa ka thekinoloji ya low-pressure casting.

Vuhumelerisi bya ti structure castings leti rharhanganeke: Hiku rharhangana ka dizayini ya swihumelerisiwa, swilaveko swale henhla swivekiwa eka vuswikoti bya thekinoloji ya low-pressure casting ku humelerisa ti structure castings leti rharhanganeke. Hiku antswisa dizayini ya xivumbeko na thekinoloji yo tata, na ku antswisa endlelo ro hoxa hi thekinoloji ya xiyimo xale henhla ya ku tekelela hi khompyuta, vuhumelerisi bya xiyimo xale henhla bya swilo swo hoxa leswingana swivumbeko leswi rharhanganeke swinene swinga fikeleriwa. Xikombiso, ku tirhisa thekinoloji yo tekelela ya khompyuta ku antswisa ndlela yo tata na endlelo ro tiya swi nga hunguta hi ndlela leyinene swihoxo eka ti castings ta xivumbeko lexi rharhanganeke na ku antswisa matirhelo ya tona na ku tshembheka.

6.2 Timhaka ta Matirhiselo ya Tithekinoloji ta Vumaki

Ku tirhisiwa ka Tisisiteme ta Vulawuri bya Vutlhari eka ku Hoxa ka Ntshikelelo wa le Hansi: Khampani leyi endlaka swiphemu swa timovha yi humese fambiselo ra vulawuri bya vutlhari ra xiyimo xa le henhla eka layini ya yona ya vuhumelerisi bya ku hoxa ka ntshikelelo wa le hansi wa aluminiyamu leyi hlanganisiweke. Sisiteme yi hlengeleta datha yo fana na ntshikelelo, mahiselo, na rivilo ro tata eka endlelo ro hoxa hi nkarhi wa xiviri hi ku nghenisa switwi swo tala swa vukheta bya le henhla eka xivumbeko na switirhisiwa, naswona yi kambisisa no swi tirhisa hi ku tirhisa tialgorithm ta xiyimo xa le henhla ku lulamisa hi ku tisungulela tipharamitha ta phurosese. Xikombiso, loko ku humelerisa ti cylinder blocks ta njhini ya movha, sisiteme ya vulawuri byo tlhariha yinga tiendlele ku antswisa rivilo ro tata na ntshikelelo wo khoma leswi seketeriweke eka data ya nkarhi wa xiviri, ku hunguta scrap rate ya ti castings hi 30%, ku engetela vuhumelerisi bya kahle hi 20%, na ku antswisa swinene swivumbeko swa michini swa ti castings, laha matimba ya tensile ya engetelekeke hi 10% - 15%.

Maendlelo ya thekinoloji ya green casting: Muendli wa swiphemu swa aerospace u tinyiketerile eka ndzavisiso na nhluvukiso na ku tirhisiwa ka thekinoloji ya green casting. Titirhisa muxaka wuntshwa wa mold coating leyinga onhiki mbango leyingana matirhelo ya kahle ya demolding xikan’we naku tiya ka mahiselo yale henhla, loko kurikarhi kuhunguta ku humesiwa ka gasi leyi nga na khombo leyi endliwaka hi swifunengeto swa ndhavuko loko switirhisiwa. Ku engetela kwalaho, khamphani yi tlhele yi endla ku cinca loku hlayisaka eneji ka switirhisiwa swo hoxa swa ntshikelelo wa le hansi, ku hunguta ku tirhisiwa ka eneji ya switirhisiwa hi 25% hi ku antswisa sisiteme yo kufumeta na ku tirhisa switirhisiwa swo pfalela leswi tirhaka kahle. Loko ku humelerisiwa ti aerospace castings letikulu, kutirhisiwa ka thekinoloji ya green casting aswi hunguti ntsena ntsengo wa vuhumelerisi, kambe switlhela swiantswisa khwalithi xikan’we naku hetisa ehenhla ka ti castings, ku fikelela swilaveko swo tika swa nsimu ya aerospace.

Nhluvukiso na ku tirhisiwa ka switirhisiwa swa aluminiyamu swa matirhelo ya le henhla: Muendli lontshwa wa mimovha ya eneji u tirhisanile na nhlangano wa ndzavisiso na nhluvukiso wa switirhisiwa ku tumbuluxa muxaka wuntshwa wa switirhisiwa swa aluminiyamu swa matirhelo ya le henhla hi ku kongoma ku humelerisa swikhegelo swa tibetiri na swikhegelo swa timovha swa mimovha leyintshwa ya eneji. Nchumu lowu wa aluminium alloy wuna matimba yale henhla xikan’we naku tiya ka corrosion yo antswa hiku engetela ti rare earth elements xikan’we naku antswisa maendlelo ya heat treatment. Loko ku tirhisiwa thekinoloji ya low-pressure casting ku humelerisa ti battery pack shells, aluminium alloy material leyintshwa yi endla leswaku matimba ya tensile ya casting ya fika eka 380-420MPa, elongation yi engeteriwa hi 20%-30%, naswona ntiko wa casting wuhungutiwa hi 10%-15%, leswi kahle kahle swi antswisaka ku tiyisela na vuhlayiseki bya mimovha leyintshwa ya eneji.

7. Swipimelo swa indasitiri na swihlawulekisi

7.1 Ku pimanisiwa ka swiyimo swa laha kaya na swa le matikweni mambe

Thekinoloji ya aluminium alloy low-pressure casting yina nxaxamelo wa swipimelo ekaya nale matikweni yale handle ku lawula maendlelo ya yona ya vuhumelerisi na khwalithi ya swihumelerisiwa. Swipimelo swa matiko ya misava swofana na ISO 945-1991 "Terms of Cast Iron Metallography", hambi leswi ngopfu ngopfu ya nsimbi leyi hoxiweke, ndlela ya nhlamuselo ya xivumbeko xa metallographic yitlhela yinyika xikombo xa nxopaxopo wa metallographic wa aluminium alloy low-pressure casting. Ku engetela kwalano, Nhlangano wa Matiko ya Misava wa Standardization (ISO) wutlhele wu humesa swipimelo swofana na ISO 8518 "Casting - Aluminium na aluminium alloy sand castings na gravity castings - Marito, tinhlamuselo na ku hlawuriwa", leswi hlamuselaka ku hlawuriwa na swilaveko swa xisekelo swa aluminium alloy castings, naswona swinyika xisekelo xa ku hlawuriwa ka low-pressure casting aluminium swirhendzevutana swa alloy.

Le Chayina, tiko ra Chayina ri tlhele ri vumba nxaxamelo wa mimpimanyeto leyi faneleke. Xikombiso, GB/T 11351-2009 "Casting aluminium alloys", leyi hlamuselaka giredi, xivumbeko xa tikhemikhali, swivumbeko swa michini na swilaveko swin'wana swa ti cast aluminium alloys, naswona yi nyika nkongomiso wa vuxokoxoko bya ku hlawuriwa ka switirhisiwa swo ka swi nga tirhisiwanga na vulawuri bya khwalithi ya aluminium alloy low-pressure casting. GB/T 13288.1-2009 "Maendlelo yo kambela ku khwaxa ka swiphemu swa ku hoxa Xiphemu xa 1: Ndlela yo pimanisa hi ku vona" yi nyika ndlela yo karhi ya ku kambela khwalithi ya le henhla ya swirhendzevutani swa ntshikelelo wa le hansi wa aluminiyamu ya alloy. Loko ku pimanisiwa na swiyimo swa matiko ya misava, swiyimo swa laha kaya Yi kongomisa ngopfu eka ku hlanganisa maendlelo ya vuhumelerisi bya laha kaya na xilaveko xa makete, naswona yi antswisa no engetela swikombiso swin’wana swo karhi swa xithekiniki na tindlela to kambela. Xikombiso, hi mayelana na vulawuri bya xivumbeko xa tikhemikhali, swipimelo swa laha kaya swi lulamise hi ndlela leyi faneleke nxaxamelo wa nhundzu ya swiaki swin’wana swa alloying leswi simekiweke eka vuhumelerisi na ku tirhisiwa ka ti alloys ta aluminiyamu ta laha kaya ku fikelela ku antswa swilaveko swa matirhelo ya ti aluminium alloy castings eka tiindasitiri to hambana ta laha kaya.

7.2 Ku tirhisiwa ka swihlawulekisi swa indasitiri

E China, ku tirhisiwa hinkwako ka swihlawulekisi eka indasitiri ya aluminium alloy low-pressure casting i swinene. Hi tlhelo rin’we, hi ku tiyisisiwa ka mphikizano wa makete, mabindzu ya le ku nyikeni nyingiso lowukulu eka ku tirhisiwa ka swiyimo swa indasitiri leswaku ku ta antswisiwa khwalithi ya swikumiwa na mphikizano wa makete. Xikombiso, leswaku ku fikeleriwa swilaveko swo tika swa ti-OEM ta mimovha eka khwalithi ya swiphemu, vaendli vo tala va swiphemu swa mimovha va landzelela hi ku hetiseka GB/T 11351-2009 na swipimelo swin’wana swa vuhumelerisi bya aluminiyamu ya aluminiyamu ya ntshikelelo wa le hansi wa ku hoxa, naswona va simeke sisiteme leyi heleleke ya vulawuri bya khwalithi ku suka eka ku xaviwa ka switirhisiwa swo ka swi nga tirhisiwanga, vulawuri bya maendlelo ya vuhumelerisi ku ya eka ku kamberiwa ka swikumiwa leswi hetiweke. Hi tlhelo rin’wana, tindzawulo ta mfumo leti faneleke ti tlhele ti tiyisisa vulawuri bya indasitiri ya ku hoxa ka ntshikelelo wa le hansi wa alloy ya aluminiyamu, na ku tlakusa mabindzu ku tirhisa hi ku hetiseka swihlawulekisi swa indasitiri hi ku tirhisa ku kamberiwa ka vulawuri bya khwalithi, vufambisi bya layisense ya vuhumelerisi na tindlela tin’wana. Xikombiso, eka malembe ya sweswinyana, tindzawulo ta vulawuri bya khwalithi ta laha kaya ti endlile ku kamberiwa ko tala ka xihatla eka vaendli va aluminiyamu ya alloy casting, ti lulamisile no xupula lava a va nga fikeleli swipimelo, naswona hi ndlela leyinene ti hlohlotele ku tirhisiwa ka mimpimanyeto ya indasitiri.

Hambiswiritano, ku tlhela ku va ni swiphiqo swin’wana. Eka mabindzu man’wana lamatsongo na ya le xikarhi, hikwalaho ka xiyimo xa xithekiniki lexi nga nyawuriki na vuvekisi bya xiphemu xa mali, ku tirhisiwa ka swiyimo swa indasitiri a swi tika hi laha ku ringaneke. Xikombiso, eka vaendli van’wana va swiphemu leswintsongo swa swithuthuthu, kungava na swiphiqo swofana naku nga kumiwi kahle ka casting surface roughness xikan’we naku pfumaleka ka vulawuri lebyi ringaneleke bya xivumbeko xa ti khemikhali. Ku engetela kwalaho, hi nhluvukiso lowu yaka emahlweni wa thekinoloji ya aluminiyamu ya aluminiyamu ya ntshikelelo wa le hansi wa ku hoxa na ku ndlandlamuxiwa ka tinsimu ta matirhiselo, swiphiqo swin’wana leswintshwa na mintlhontlho swi tlhele swi veka emahlweni swilaveko swa le henhla swa ku tirhisiwa ka mimpimanyeto ya indasitiri leyi nga kona. Xikombiso, eka xiyenge xa ​​mimovha leyintshwa ya eneji, swilaveko swa ku olova na matirhelo ya le henhla ya swirhendzevutani swa ntshikelelo wa le hansi swa aluminiyamu alloy swi ya swi tlakuka, naswona swa laveka ku ya emahlweni ku antswisiwa swiyimo leswi faneleke na swihlawulekisi ku kongomisa ku antswa maendlelo ya vuhumelerisi bya mabindzu.